Specification |
Type: Oriented Silicon Steel;
Standard: GB;
Technique: Cold Rolled;
Shape: Sheet;
Thickness: 0.20mm;
Iron Loss: 0.65W/Kg(1.7t/50Hz);
Brand: Julong;
Width: 35-1060mm;
Transformer Lamination: OEM(According to Drawing);
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|